Grosir Rigging Rantai Angkat Hoist Baja Paduan G80
Grosir Rigging Rantai Angkat Hoist Baja Paduan G80
Kategori
Ngangkat sareng ngiket, ranté, ranté tautan pondok, ngangkat ranté tautan buleud, ranté Kelas 80, ranté G80, sling ranté, ranté sling, ranté toleransi sedeng DIN 818-2 pikeun sling ranté Kelas 8, ranté baja paduan
Aplikasi
Ngangkat jeung ngiket, ngangkat beban, ngabeungkeut beban
Ranté SCIC Grade 80 (G80) pikeun ngangkat didamel numutkeun standar EN 818-2, nganggo baja paduan mangan nikel kromium molibdenum numutkeun standar DIN 17115; las & perlakuan panas anu dirancang / diawasi kalayan saé mastikeun sipat mékanis ranté kalebet gaya uji, gaya putus, elongasi & karasa.
Gambar 1: Diménsi ranté kelas 80
meja 1: Kelas 80 (G80) dimensi ranté, EN 818-2
| diaméterna | lapangan | lébar | beurat hijian | |||
| ngaran | kasabaran | p (mm) | kasabaran | W1 jero | W2 luar | |
| 6 | ± 0.24 | 18 | ± 0.5 | 7.8 | 22.2 | 0.8 |
| 7 | ± 0.28 | 21 | ± 0.6 | 9.1 | 25.9 | 1.1 |
| 8 | ± 0.32 | 24 | ± 0.7 | 10.4 | 29.6 | 1.4 |
| 10 | ± 0.4 | 30 | ± 0.9 | 13 | 37 | 2.2 |
| 13 | ± 0,52 | 39 | ± 1.2 | 16.9 | 48.1 | 4.1 |
| 16 | ± 0,64 | 48 | ± 1.4 | 20.8 | 59.2 | 6.2 |
| 18 | ± 0.9 | 54 | ± 1.6 | 23.4 | 66.6 | 8 |
| 19 | ± 1 | 57 | ± 1.7 | 24.7 | 70.3 | 9 |
| 20 | ± 1 | 60 | ± 1.8 | 26 | 74 | 9.9 |
| 22 | ± 1.1 | 66 | ± 2.0 | 28.6 | 81.4 | 12 |
| 23 | ± 1.2 | 69 | ± 2.1 | 29.9 | 85.1 | 13.1 |
| 24 | ± 1.2 | 72 | ± 2.1 | 30 | 84 | 14.5 |
| 25 | ± 1.3 | 75 | ± 2.2 | 32.5 | 92.5 | 15.6 |
| 26 | ± 1.3 | 78 | ± 2.3 | 33.8 | 96.2 | 16.8 |
| 28 | ± 1.4 | 84 | ± 2.5 | 36.4 | 104 | 19.5 |
| 30 | ± 1.5 | 90 | ± 2.7 | 37.5 | 105 | 22.1 |
| 32 | ± 1.6 | 96 | ± 2.9 | 41.6 | 118 | 25.4 |
| 36 | ± 1.8 | 108 | ± 3.2 | 46.8 | 133 | 32.1 |
| 38 | ± 1.9 | 114 | ± 3.4 | 49.4 | 140.6 | 35.8 |
| 40 | ± 2 | 120 | ± 4.0 | 52 | 148 | 39.7 |
| 45 | ± 2.3 | 135 | ± 4.0 | 58.5 | 167 | 52.2 |
| 48 | ± 2.4 | 144 | ± 4.3 | 62.4 | 177.6 | 57.2 |
| 50 | ± 2.6 | 150 | ± 4.5 | 65 | 185 | 62 |
Tabel 2: Sipat mékanis ranté Kelas 80 (G80), EN 818-2
| diaméterna | wates beban kerja | kakuatan bukti manufaktur | gaya pegat minimum |
| 6 | 1.12 | 28.3 | 45.2 |
| 7 | 1.5 | 38.5 | 61.6 |
| 8 | 2 | 50.3 | 80.4 |
| 10 | 3.15 | 78.5 | 126 |
| 13 | 5.3 | 133 | 212 |
| 16 | 8 | 201 | 322 |
| 18 | 10 | 254 | 407 |
| 19 | 11.2 | 284 | 454 |
| 20 | 12.5 | 314 | 503 |
| 22 | 15 | 380 | 608 |
| 23 | 16 | 415 | 665 |
| 24 | 18 | 452 | 723 |
| 25 | 20 | 491 | 785 |
| 26 | 21.2 | 531 | 850 |
| 28 | 25 | 616 | 985 |
| 30 | 28 | 706 | 1130 |
| 32 | 31.5 | 804 | 1290 |
| 36 | 40 | 1020 | 1630 |
| 38 | 45 | 1130 | 1810 |
| 40 | 50 | 1260 | 2010 |
| 45 | 63 | 1590 | 2540 |
| 48 | 72 | 1800 | 2890 |
| 50 | 78.5 | 1963 | 3140 |
| catetan: total elongasi pamungkas dina gaya pegat nyaéta minimum 20%; | |||
| parobahan Wates Beban Kerja dina hubunganana sareng suhu | |
| Suhu (°C) | % WLL |
| -40 nepi ka 200 | 100% |
| 200 nepi ka 300 | 90% |
| 300 nepi ka 400 | 75% |
| leuwih ti 400 | teu bisa ditarima |